In the production of flexible packaging lamination, poor friction resistance of the finished product, transportation friction-induced ink layer wear and blurring, and ink layer detachment are common functional defects. Many products have normal bonding strength and no delamination or blistering, but the abrasion test fails to meet the standards. After batch production, due to surface abrasion and color fading, customer complaints occur, especially for large-area colored printing films and matte films, which are more prominent and seriously affect the product appearance and the qualification rate of shipment.
 
Insufficient interfacial adhesion is the core reason for poor wear resistance. Residual ink dust, silicone oil, release agents, and static dust on the surface of the printing film will form a barrier layer between the ink and the adhesive, preventing the Polyurethane Adhesive from closely penetrating the ink layer. After bonding, the adhesive and ink bonding strength is weak, and when subjected to external friction, the adhesive layer and ink layer are prone to peel and slide, resulting in blurring, ink loss, and frosting.
laminating adhesive
Improper selection of process parameters will exacerbate the wear defect. Low coating dryness and thin adhesive layer cannot form a tough protective film, and the surface layer is prone to wear after being stressed; incomplete adhesive curing and insufficient crosslinking density lead to a soft adhesive layer and a significant reduction in wear resistance. At the same time, insufficient curing time and low temperature also result in loose adhesion at the adhesive-ink interface, which is also an important cause of poor friction.
 
On-site improvement should be implemented in both interface treatment and process optimization. Before bonding, clean the dust and impurities on the surface of the printing film to ensure a clean and dry ink layer, and improve the adhesion of the adhesive. Reasonably match the coating dryness to ensure a full and dense adhesive layer, forming a good protective layer. Strictly control the mixing ratio and curing parameters to ensure complete crosslinking of the adhesive layer and a firm and stable gel. Through standardized control, the friction resistance of the composite film can be significantly improved, and the problems of frosting and ink loss can be eliminated.
Contact Us

Author:

Ms. Cherry

Phone/WhatsApp:

+86 13549820808

Popular Products
You may also like
Related Categories

Email to this supplier

Subject:
Mobile:
Email:
Message:

Your message must be between 20-8000 characters

Copyright © 2026 Guangdong Xinhui Chemical Co.,Ltd. All rights reserved. Privacy Policy

We will contact you immediately

Fill in more information so that we can get in touch with you faster

Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.

Send